imported_Ivan Rajic
New member
RZJZA80 said:it seems like 105 is used on every single car nowadays, no matter what level of correction it really needs, of course that can't really be the case. So with that being said, what are the best options for just some swirl marks or light marring? Is Megs 83 still the go to for lighter cut and 105 for everything else?
RZJZA80 said:No I agree with you, although most won't admit it, it does seem as if 105 is automatically used no matter what
I guess an argument that would make sense here is PC vs rotary... it's obvious that when using the PC M105 helps a lot in defect correction but I still feel there isn't a need for it that much, especially with the rotary... I made this moreso to reflect PC usage because I am positive with some pressure the PC can remove more paint than rotary with same pad/polish, and with M105, it can become too much too fast... M83 is still a very good cutting step followed by M80 or the new M205