ProStreetCamaro
New member
I polished out my hood to perfection to test csl topped with exov2. Well apparently my microfiber i used to wipe the excess product off must have had a speck of something hard on it and it put light swirl like scratches all over the hood. They are very light and you can only see them in direct sun light but being a little OCD about my Grand cherokee srt makes me want to polish it back out and do the hood over. I am wondering how hard it is to remove CSL? I know crystal serum pro has to be sanded but how hard is CSL? Will a UHS pad and UHS polish be enough or would something like M105 and a rupes blue microfiber pad be needed?
P.S. I washed my truck today for the first time since doing the hood a few days ago. EXOV2 is the most hydrophobic coating I have ever seen. Absolutely incredible!
P.S. I washed my truck today for the first time since doing the hood a few days ago. EXOV2 is the most hydrophobic coating I have ever seen. Absolutely incredible!