Hello everyone. It was a HOT day again in MN with temps in my garage hitting upper 90's for the 3rd day in a row. I have to keep the doors close becuase of all the fuzzies blowing in all over the car.

Carpets

Vacuum
APC 20:1
Folex
Agitate
Extract

halfmat.jpg


Vinyl and Plastics

APC 20:1
VRT
Wipe with MF after an hour


Exterior

Was in good condition so it needed only minimal polishin other than the hood.

NXT
Clay with NXT wash as lube
2.5 on hood only/ LC 7.5" lightcut pad/PC
DP mild swirl remover/ LC 7.5" polishing pad/PC
PwC via hand on headlights too
Pinnacle Sig via hand

rightrear.jpg


leftrear.jpg


hood.jpg


front.jpg



Engine

APC 10:1 let dwell for 5 minutes
agitate with various baja sol brushes
spray down
run engine for 5-10 mintues
No Touch Aerosol Protectant
Wipe after 3 hours

engine.jpg


Greg
 
6 hours. It was really hard to get a nice shine like im used to becuase of the enormous amount of flake the car had.

Greg
 
Nice work Greg! :bigups

That is a tough color to get some "POP"... you did a nice job getting some!
 
I was in a bit of a rush so I didnt get to S+G. It is a freind of the families car so im going back next week to S+W, pin sig, and S+G x 2. I will post some pics if I get any more pop from the S+G.

Greg
 
Back
Top