The Guz
Mike
It has been a little over a month and I am already starting to see some changes in hydrophobics with the car sitting outside 24/7.
Best Self cleaning effect: (Top 5)
Gyeon Syncro. As I mentioned from previous experience its initial performance is top notch. Lets see is it holds out or fizzles out in about 5 months total when Skin starts to show signs of degradation.
SPS Graphene
Cquartz UK 3.0
IGL
Adams UV Ceramic
Loss of hydrophobics.
Drexler Ceramic (Base Coat + Top Coat) - this has turned into sheeting like Gyeon Mohs. Water lays flat on the surface. Seems like it is either an application issue or the top coat is indeed already degrading.
Adams UV Spray Coating - This showed signs of slowing down after the first wash. It has one of the worst self cleaning effects. Turning into sheeting.
Cquartz TiO2 - This has started to turn into sheeting and its water beading has started to become more oblong shape. I believe this is looking like an application error as I have experienced this to perform on par with CQUK 3.0 on my hood for the last 20 months. It is not the first time I see application inconsistencies with it. I am going to leave it for now but I am to the point where I will not be focusing too much on it and will include is with test #2 next year.
The remaining coatings seem to be doing fine.
Best Self cleaning effect: (Top 5)
Gyeon Syncro. As I mentioned from previous experience its initial performance is top notch. Lets see is it holds out or fizzles out in about 5 months total when Skin starts to show signs of degradation.
SPS Graphene
Cquartz UK 3.0
IGL
Adams UV Ceramic
Loss of hydrophobics.
Drexler Ceramic (Base Coat + Top Coat) - this has turned into sheeting like Gyeon Mohs. Water lays flat on the surface. Seems like it is either an application issue or the top coat is indeed already degrading.
Adams UV Spray Coating - This showed signs of slowing down after the first wash. It has one of the worst self cleaning effects. Turning into sheeting.
Cquartz TiO2 - This has started to turn into sheeting and its water beading has started to become more oblong shape. I believe this is looking like an application error as I have experienced this to perform on par with CQUK 3.0 on my hood for the last 20 months. It is not the first time I see application inconsistencies with it. I am going to leave it for now but I am to the point where I will not be focusing too much on it and will include is with test #2 next year.
The remaining coatings seem to be doing fine.