512detail
New member
3 days shy of 5 months on the hood
see: http://www.autopia.org/forums/detai...oly-sheet-exo-csl-csl-exo-longevity-test.html
for details
so long story short at around 4 months I noticed the exo v2 side grew a bald spot and started losing it`s nice beads as well so I topped it with PA high gloss, which apparently didn`t stick to the exov2 because it made essentially no water behavior difference when I washed a few weeks later or it just washed off perhaps
I since have used Ech20 as drying aid and it brought back some of the water behavior (well, i guess technically it iust provided some beading until it wears off)
Guz suggested it was time for a decon wash so I had some spare time this AM and its supposed to rain so I figured why not
rinsed hood and sprayed BDX generously all over hood
let sit for a few mins and wiped in with a wash mitt and then rinsed off
well it brought back some good sheeting to CSL, seems to have unaffected the csl+exov2 much but nothing was wrong with it
it also brought back the exov2s bald spot
hope the vid loads of after bdx wash
https://vimeo.com/199554806
csl + exov2
csl middle
exov2 left
i cant get the vids to load and if i get motivated later i will upload them to and embed from youtube
but the exov2 was clearly in last place, csl somewhat cane back to life, sheeting wise only, and csl+exov2-well that stuff is still as ridiculous as day 1...but its killing me because I want to top ot and nothing will make it any better, only probably worse as ive seen with topping it in the pasr, it takes away some of the very high contact angle on the beads
well i just couldnt look at this anymore
enter PBL coating booster applied to both the exov2 and csl only parts
and hello beads and fast sheeting again
exov2 only side left
csl middle
csl + exov2 right
im hoping this vid below loads of the hood after pbl on the two independent exov2 and csl sections
https://vimeo.com/199554626
thanks for viewing
-Brandt K.
see: http://www.autopia.org/forums/detai...oly-sheet-exo-csl-csl-exo-longevity-test.html
for details
so long story short at around 4 months I noticed the exo v2 side grew a bald spot and started losing it`s nice beads as well so I topped it with PA high gloss, which apparently didn`t stick to the exov2 because it made essentially no water behavior difference when I washed a few weeks later or it just washed off perhaps
I since have used Ech20 as drying aid and it brought back some of the water behavior (well, i guess technically it iust provided some beading until it wears off)
Guz suggested it was time for a decon wash so I had some spare time this AM and its supposed to rain so I figured why not
rinsed hood and sprayed BDX generously all over hood

let sit for a few mins and wiped in with a wash mitt and then rinsed off
well it brought back some good sheeting to CSL, seems to have unaffected the csl+exov2 much but nothing was wrong with it
it also brought back the exov2s bald spot
hope the vid loads of after bdx wash
https://vimeo.com/199554806




i cant get the vids to load and if i get motivated later i will upload them to and embed from youtube
but the exov2 was clearly in last place, csl somewhat cane back to life, sheeting wise only, and csl+exov2-well that stuff is still as ridiculous as day 1...but its killing me because I want to top ot and nothing will make it any better, only probably worse as ive seen with topping it in the pasr, it takes away some of the very high contact angle on the beads
well i just couldnt look at this anymore

enter PBL coating booster applied to both the exov2 and csl only parts

and hello beads and fast sheeting again


exov2 only side left


im hoping this vid below loads of the hood after pbl on the two independent exov2 and csl sections
https://vimeo.com/199554626
thanks for viewing
-Brandt K.