Sep 13, 2005 #1 0 03k20a2 New member well i ordered some mf bonnets and had to order a lambswool pad 60/40, not 100 wool. does anyone use this wool pad for compounding if a yellow lake county pad is not cutting it? i was just curious
well i ordered some mf bonnets and had to order a lambswool pad 60/40, not 100 wool. does anyone use this wool pad for compounding if a yellow lake county pad is not cutting it? i was just curious
Sep 13, 2005 #2 I imported_drg New member ive used a wool pad on a pc with mother power polish, no hazing worked really well, even at speed 6 with alot of pressure
ive used a wool pad on a pc with mother power polish, no hazing worked really well, even at speed 6 with alot of pressure
Sep 14, 2005 #3 A Accumulator Well-known member I used wool pads with the PC and 3M FCRC. The wool wasn't really much more aggressive than a yellow cutting pad. But all wool pads are *not* the same.
I used wool pads with the PC and 3M FCRC. The wool wasn't really much more aggressive than a yellow cutting pad. But all wool pads are *not* the same.
Sep 14, 2005 #4 I imported_kgb New member I used one once and it left a bunch of DA marks in the paint I had to go back over with a foam pad to remove.
I used one once and it left a bunch of DA marks in the paint I had to go back over with a foam pad to remove.
Sep 14, 2005 #5 4830Deuce Burn Then Buff! I did once...The only time I would really think about using one with a PC is after wetsanding to level out the paint...
I did once...The only time I would really think about using one with a PC is after wetsanding to level out the paint...