FP2 micromarring?

wannafbody

wannafbody
I've been playing around with FP2 with both the Megs Tan finishing pad and the green german foam CMA CCS pad. I'm getting what looks like very fine circular micromarring. Are these pads too soft or am I just not working the product long enough? Any one else experience this?
 
When I first started using FPII, I noticed the same thing. I believe I was not working the polish in enough. I was using a White CMA CCS pad. Worked it in a little while longer and the marring was gone.
 