Used my new PC 7336 and lake country pads today with SSR2 (orange pad) and SSR1(white pad) and finished with Gold Class wax (grey pad). Swirl marks were reduced by 75% I would say (may need to use SSR2.5), but I have some other marks now. Not sure what to call them....micromarring?? They look like they came from the PC. Do you think I used the right pads with the products listed? I put 5 or 6 dime sized "dallops" on the pad for each 2X2 area....to much, not enough? What sort of time frame for each section...1 minute, 2? Any suggestions..........
.....paint is a dark blue on a F-150