DP finish polish/Klasse AIO/SG/EX-P

emaxxman

New member
Can I use DP Final Finishing Polish under Klasse SG? It says it doesn't contain any fillers so I'm assuming it won't hinder adherence or durability of SG. Is that correct?



I like the DP because it's much more economical than AIO right now.



Also, I'm still debating on which sealant to get. Originally, I wanted to go with Klasse for it's incredible durability. But I'm leaning towards EX-P for its ability to be used in full sun.



Here are my choices that I've narrowed it down to:



1. Klasse AIO and SG

2. DP FFP and Klasse SG (will this have reduced durability compared to choice #1)

3. DP FFP and Poorboy's EXP

4. Klasse AIO and EXP (this probably really isn't a choice but I put it here anyway.)



Has anyone compared the durability of SG and EXP? If so, what did you find?

Has anyone used FFP under SG?



I settled on FFP or AIO as I want a non-abrasive polish. I've already got DACP and Speed Glaze for abrasives.
 
Yes, you can do the finishing polish under SG, but just to be safe do a 50/50 Isopropyl Alcohol/Water wipe down. You might(probably) not get full durability of the SG if it is not used over AIO. EX-P has pretty crappy durability, IMO. I only get 2.5 months max out of it. SG should last for 5 or 6 months. Just to be safe I would do AIO and SG, and if you wanted to you could go FFP-AIO-SG.
 
Also, I was also thinking of using Optimum's wax over whichever sealant I use. I figured the wax could be the sacrificial layer and also be an easily rejuvenated shine coat. Would OCW remove the sealant? I didn't see any cleaners mentioned in it so I don't think it will but just want to make sure.
 
No, OCW will not compromise the underlying layer of product.



Try Duragloss Aquawax, I have used it and it is super slick and very clear and wet.
 
Back