    I do restoration paint jobs in my spare time as a hobby and a way to make extra money. I get good results when I cut and buff but I`m looking to perfect my buffing skills because I believe it will help me take my work to the next level. Most of the discussion on this forum is aimed at paint correction of factory paint that has been neglected over time which is very different from the paint that I work on. When it`s all said and done I will have 5-6 coats of clear on the car and usually wetsand with 1500 then 3000 before buffing, and I have been using Menzerna compounds/polishes with Lake Country CCS pads. The clear I use is very soft and buffs easily.



    Questions:



    I usually start my sanding with 1500 on a DA. Sometimes I have a little more orange peel in some areas vs others so I have to spend more time sanding there to get it out. It seems like in these spots I end up with a bit of a ripple effect when looking at reflections once I get it all polished up. I assume this is because although the panel and paint are flat, the clear is not due to the sanding with the DA. I am thinking about starting my sanding on this next car with 1000 on a block to get all the orange peel out and then moving to the DA. Will I be ok to go with 1500 to get the 1000 scratches out you think, or maybe 1200? Maybe 1000 to start with is too much? By the way, I plan to use Megs Unigrit 1000 and then I`m gonna try the Norton Dry Ice system on the DA since I read a good post about it here recently.



    Once I get the clear flat with the sanding, I`m ready to bring the shine back. The car I have in the shop right now is black and I`m looking to get the best gloss/depth possible. How much of this is going to be the products I use vs just having good technique? If I get the clear perfectly flat with the sanding, then remove all the sanding by compounding and then remove any defects of compounding with polish, the surface of the clear should be perfect and defect free, but can getting it defect free with one group of products vs another make a difference in the final appearance? This is the real questions I`m hoping to get answered because I`ve only used Menzerna`s stuff and I`ve always wondered if I`m missing out on something.

  2. #2
    CCH Auto Appearance, LLC C. Charles Hahn's Avatar
    Join Date
    Jul 2003
    Location
    Lansing, MI USA
    Posts
    8,783
    Post Thanks / Like
    With 5-6 coats of total clear to work with you should be perfectly fine starting at 1000 grit and moving to 1500 and then 3000 from there. I too have heard some good things about Norton`s Liquid Ice system and know a few painters who recommend it, but depending on how fresh the paint is when you`re buffing it I wouldn`t recommend using a DA. And, to be honest, I question if the Norton system (I`ve never used it personally, but based on what I`ve seen) will really give you better results than the Menzerna you`re already using.



    Unlike with a sanding disc, a polishing pad has the tendency to grab at the surface and could cause "paint wrinkle" as a result of the DA`s motion pattern. On fresh paint it`s better to stick with a rotary as a rule.



    What specific Menzerna polishes are you using? And what are you finishing with? 85RD, 106FA, or something else?
    Charlie
    Automotive Appearance Specialist - Serving Greater Lansing, Michigan
    http://www.cchautoappearance.com/

  3. #3

    Join Date
    Aug 2012
    Posts
    2,059
    Post Thanks / Like
    You should definitely be able to start with 1000 grit, then 1500 then 2000 and if you want finish with 3000. I would stick with Menzerna polishes, but you may want to try blocking the pain instead of a d.a. It should finish out even flatter.





    John

  4. #4
    CCH Auto Appearance, LLC C. Charles Hahn's Avatar
    Join Date
    Jul 2003
    Location
    Lansing, MI USA
    Posts
    8,783
    Post Thanks / Like
    Quote Originally Posted by JohnKleven
    You should definitely be able to start with 1000 grit, then 1500 then 2000 and if you want finish with 3000. I would stick with Menzerna polishes, but you may want to try blocking the pain instead of a d.a. It should finish out even flatter.





    John


    John, sorry but I don`t agree. First there`s really no need for the added step of 2000 grit if he`s working via DA, going straight from 1500 to 3000 is fine. Second, I don`t know where you`re getting that blocking by hand will finish out flatter than using a DA -- if anything the DA gives you a more consistent bed of sanding marks with less chance of instilling deeper tracers.
    Charlie
    Automotive Appearance Specialist - Serving Greater Lansing, Michigan
    http://www.cchautoappearance.com/

  5. #5

    Join Date
    Sep 2009
    Posts
    454
    Post Thanks / Like
    :xyxthumbs
    Richie Carbone
    Richie`s Custom Detailing
    Advanced Paint Correction Detail Services
    Specializing in Luxury & Exotic Autos

    Serving Cental & South Florida

  6. #6

    Join Date
    Sep 2009
    Posts
    454
    Post Thanks / Like
    Quote Originally Posted by Shiny Lil Detlr
    John, sorry but I don`t agree. First there`s really no need for the added step of 2000 grit if he`s working via DA, going straight from 1500 to 3000 is fine. Second, I don`t know where you`re getting that blocking by hand will finish out flatter than using a DA -- if anything the DA gives you a more consistent bed of sanding marks with less chance of instilling deeper tracers.


    :xyxthumbs
    Richie Carbone
    Richie`s Custom Detailing
    Advanced Paint Correction Detail Services
    Specializing in Luxury & Exotic Autos

    Serving Cental & South Florida

  7. #7

    Join Date
    May 2011
    Location
    Herne Bay, Kent, United Kingdom
    Posts
    4
    Post Thanks / Like
    Quote Originally Posted by Shiny Lil Detlr
    John, sorry but I don`t agree. First there`s really no need for the added step of 2000 grit if he`s working via DA, going straight from 1500 to 3000 is fine. Second, I don`t know where you`re getting that blocking by hand will finish out flatter than using a DA -- if anything the DA gives you a more consistent bed of sanding marks with less chance of instilling deeper tracers.
    :xyxthumbs:xyxthumbs
    Applying the shine one day at a time

    http://www.aclassvaleting.net

    Herne bay kent UK

  8. #8

    Join Date
    Feb 2008
    Posts
    11
    Post Thanks / Like
    What specific Menzerna polishes are you using? And what are you finishing with? 85RD, 106FA, or something else?


    I have Power Gloss, SIP, and 106FA. I think I may get some PO85RD to try out as well. I read a lot of good things about it and I believe it should get me a little more gloss than the 106FA.



    I too have heard some good things about Norton`s Liquid Ice system and know a few painters who recommend it, but depending on how fresh the paint is when you`re buffing it I wouldn`t recommend using a DA. And, to be honest, I question if the Norton system (I`ve never used it personally, but based on what I`ve seen) will really give you better results than the Menzerna you`re already using.


    I was going to DA with the sanding discs, and buff with rotary, only gonna use DA to finish buffing if I need to. Also, I was talking about the Dry Ice sanding discs, not the liquid ice compound.





    I see what John is saying and I have to say it makes a lot of sense to me. When I spray a car some spots have more orange peel than others. If I use a block and wetsand by hand until all the orange peel is out I should have a level coat of clear over the whole car. Then I could get after it with the 1500 on the DA and remove the sanding marks and any tracers created while blocking. When starting with the DA to remove orange peel I think I often create an uneven surface. Although all the orange peel is out there are very subtle waves in the clear, and that`s what I want to avoid.

  9. #9

    Join Date
    Aug 2012
    Posts
    2,059
    Post Thanks / Like
    Nope. A d.a. Is NOT as flat as blocking, especially if you`re using an intermediate pad onyour d.a. I do probably 10+ full car sands per year, some I do dry with d.a. Som

    wet with a block. The D.A. Cuts the time dramatically, but will never finish as flat. You won`t find a d.a. Being used on big money hot rods.



    I like to go from 1500-2000 as it makes for an easier polish in my opinion.





    John

  10. #10

    Join Date
    Feb 2008
    Posts
    11
    Post Thanks / Like
    So you`re saying no DA at all huh? That would take some time for sure.

  11. #11
    CCH Auto Appearance, LLC C. Charles Hahn's Avatar
    Join Date
    Jul 2003
    Location
    Lansing, MI USA
    Posts
    8,783
    Post Thanks / Like
    Quote Originally Posted by transamfan
    So you`re saying no DA at all huh? That would take some time for sure.


    John is welcome to his opinion of course, but to be honest I`ve talked to a few darn good painters and while they do use hand sanding techniques for certain jobs, they do the majority of their work via DA.



    I guess if you can find the combination of techniques that works best for you (maybe 1000 grit by hand, then 1500 and 3000 via DA) that`s what is most important.



    All that said, while I do not have any experience with the Norton Dry Ice abrasives you mentioned, I will say that I use Meguiar`s Unigrit abrasives pretty much exclusively (3M Imperial Wetordry if I run out in the middle of a job in a pinch, but that`s rare) and I`ve always been happy with the results.
    Charlie
    Automotive Appearance Specialist - Serving Greater Lansing, Michigan
    http://www.cchautoappearance.com/

  12. #12

    Join Date
    Aug 2012
    Posts
    2,059
    Post Thanks / Like
    I`m not saying no DA. I`m saying a DA is not as flat as a block. I use a DA regularly, actually I used one today. There is a reason why people long block bodywork before paint, which takes much more time, but looks way better than a DA. The same applies before the paint is applied, and after.

  13. #13
    Forza Auto Salon David Fermani's Avatar
    Join Date
    Aug 2004
    Location
    Troy, MI
    Posts
    12,534
    Post Thanks / Like
    Quote Originally Posted by JohnKleven
    I`m not saying no DA. I`m saying a DA is not as flat as a block. I use a DA regularly, actually I used one today. There is a reason why people long block bodywork before paint, which takes much more time, but looks way better than a DA. The same applies before the paint is applied, and after.


    That`s 2 totally different applications all together. Bodywork, because you`re using MUCH coarser abrasives, requires blocking to ensure the appearance of perfect flatness. Sanding the clear that goes on top with a MUCH finer abrasive does not. The key to doing full wet sands above and beyond applying additional coats of clear(on bccc) is the initial removal of heavy media which can quickly and effectively be done with a DA. After that you`re basically refining your scratches. The more refinement your choose to do, the less need is required for heavy compounding.
    Metro Detroit`s leader in cleaning, preserving & perfecting fine automobiles!

  14. #14

    Join Date
    Aug 2012
    Posts
    2,059
    Post Thanks / Like
    Quote Originally Posted by David Fermani
    That`s 2 totally different applications all together. Bodywork, because you`re using MUCH coarser abrasives, requires blocking to ensure the appearance of perfect flatness. Sanding the clear that goes on top with a MUCH finer abrasive does not.


    I agree with you David to a point, as your statement is true. However, why not finish the CC to the same level as the bodywork, meaning to shear the orange peel off. This will eliminate any waviness in the paint, that can come from DA sanding. I may be overanalyzing this, but for someone like myself, who is very passionate about creating a perfect finish, I`m talking about 5%. Blocking takes more time, and both methods can and will provide incredible results, but I think blocking gives you that extra 5%.

  15. #15
    Forza Auto Salon David Fermani's Avatar
    Join Date
    Aug 2004
    Location
    Troy, MI
    Posts
    12,534
    Post Thanks / Like
    Again, flat body work is on a totally different level than the flat outer surface. Mainly because your base(primer) is finished in much coarser abrasives. Especially seeing that clear coat is typically the thickness of a single sheet of paper. External waviness comes from incorrect removal of the surface (i.e. orange peel). As long as that has been done, I really don`t believe anyone`s eye can pick up a variance measured in single digit microns. It goes beyond passion at that point. In most extreme cases, to create a "perfect" finish, besides removal of orange peel, the base requires extensive blocking in between coats too. Now that`s a noticeable difference.
    Metro Detroit`s leader in cleaning, preserving & perfecting fine automobiles!

 

 
Page 1 of 5 12345 LastLast

Thread Information

Users Browsing this Thread

There are currently 1 users browsing this thread. (0 members and 1 guests)

Similar Threads

  1. help with buffing after wetsanding
    By sweetextreme in forum Wetsanding For A Show Car Shine
    Replies: 25
    Last Post: 05-12-2011, 12:42 AM
  2. wetsanding question fresh paint
    By lex99frc in forum Car Detailing
    Replies: 15
    Last Post: 05-14-2009, 12:33 PM
  3. Wetsanding after fresh painting
    By LandonZ in forum Professional Detailer General Discussion
    Replies: 4
    Last Post: 04-25-2007, 11:40 AM
  4. Wetsanding/Buffing Class in MA Feb 10
    By SuperBuick in forum Northeast USA
    Replies: 8
    Last Post: 02-12-2007, 03:13 PM
  5. Fresh From Paint, Wetsanding to Follow
    By imported_dpeezy415 in forum Click & Brag -The Detailers Showcase
    Replies: 7
    Last Post: 05-01-2005, 02:35 PM

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts
  •