Originally Posted by
Stokdgs
Hello Scrapyard !
In my experience, glazes are always something that is applied -after- the correction stage/s, and is only going to help hide any very minor issues that were not solved during the correction stage..
We used those things 50 years ago in the Paint Shop I was working in. And only after correction was completed, to give the paint an even more smooth, slick, wet-paint-look..
The product of choice was Meguiars Nbr-7 Glaze..
Believe that any hard working of a glaze will only heat it up too much, and cause it to do weird things in the paintwork, as what happened to you..
I believe that Jescar product you used might have been called Menzerna PowerLock Polymer Sealant, a long time ago, no ? If it is in fact the case, I still have that Menzerna product and I only used it after all the correction work was done and the Client did not want anything else more expensive done to the Paintwork.. It was applied by hand, looked great, probably lasted a few weeks, and then was gone..
Dan F