Do you mean to tell me coatings are not fire proof?
The coating and polish are pretty straight forward. Nothing to really say here. I still prep wipe with Essence and have had no issues doing that.
I would not even bother with Reload unless the coating is going to see rain right away.
You are familiar enough with CSL. Only thing to mention is stick with 1 layer as that is all that is needed. The directions and even Gtechniq`s site mention one can apply Exo right after CSL but I am now hearing from installers that it is recommended to let CSL cure for 4-6 hours prior to applying Exo. With Exo one can reapply the second layer right after the first one is done. Essentially start at the same place you started with the first layer.
One thing with Exo V3 and I am not sure if V4 is the same, is that the coating is pushed around on the surface and requires multiple towels. You may want to use 3 towels at a time and wipe larger areas to make sure it is completely off the surface to avoid high spots.
Nice. My Pro2 just came in with some VS1 as well. So it will be interesting to see your observations as well. I may give 3D One a go as I just got that but have not had a chance to try it out. I may use Shine Supply`s primer polish as a base as well.
Looking forward to seeing if this coating lives up to the hype. Especially with the self healing aspects.