Here are some photos of a boat I`m doing for a buddy. It`s a 1971 Sea Ray Pachanga jet drive boat that was in storage for many years.
Hull was very chalky and dull on the horizontal surfaces.
Process:
3M Marine Compound, wool compounding pad, 2200 rpm
That didn`t do it, still a lot of chalkiness, so wet sand a little
Repeat compunding step, a few passes.
3M Finesse-It Finishing Material, Blue Edge foam, 1500 rpm.
Meguiars Flagship wax, LC white pad, PC, speed 4
Before:
http://www.autopia.org/gallery/data/500/Before5.jpg
During:
http://www.autopia.org/gallery/data/500/During_looking_fwd.jpg
http://www.autopia.org/gallery/data/500/Durin_looking_aft1.jpg
Afters:
http://www.autopia.org/gallery/data/500/After_looking_fwd.jpg
http://www.autopia.org/gallery/data/500/After_looking_aft.jpg
http://www.autopia.org/gallery/data/500/After_reflection.jpg
Hull was very chalky and dull on the horizontal surfaces.
Process:
3M Marine Compound, wool compounding pad, 2200 rpm
That didn`t do it, still a lot of chalkiness, so wet sand a little
Repeat compunding step, a few passes.
3M Finesse-It Finishing Material, Blue Edge foam, 1500 rpm.
Meguiars Flagship wax, LC white pad, PC, speed 4
Before:
http://www.autopia.org/gallery/data/500/Before5.jpg
During:
http://www.autopia.org/gallery/data/500/During_looking_fwd.jpg
http://www.autopia.org/gallery/data/500/Durin_looking_aft1.jpg
Afters:
http://www.autopia.org/gallery/data/500/After_looking_fwd.jpg
http://www.autopia.org/gallery/data/500/After_looking_aft.jpg
http://www.autopia.org/gallery/data/500/After_reflection.jpg