Re: Midwest Winter Prep Follow-up Question: Top UPGP with 845 or FK1000P?

Quote:
Originally Posted by slawek65 View Post
I think ( from search FK 1000P - I can be wrong ) 1000P have cure time 30 min so You can have 2coats of 1000P in 1hr. Don't top with 845,845 have lots of solvent and can remove 1-st coat. Again I can be wrong.
I have seen many more posts claiming fk1000p can be layerd after 30 mins to an hour than I have seen reporting it needs 24 hr cure time. I would give a coat of the UPGP followed next day by a coat of fk1000p. I wouldnt expect any problems with 1000p bonding over UPGP.
  Reply With Quote